Hastelloy C276 Sheet
1. Standard: ASTM B575, ASTM B333, ASTM B906
2. Width: 0~2500mm or Customized
3. Length: 0~12m or Customized
4. Thickness: 0.3~ 20mm or Customized
5. Grades:Hastelloy c276, UNS N10276, EN 2.4819
Hastelloy c276 sheet has strong resistance to chloride stress corrosion cracking, pitting, crevice corrosion and general corrosion. Because of the addition of high molybdenum and chromium content and tungsten. nickel alloy C-276 sheet thickness ranges from 3/16 inch (4.8 mm) to 2 ½ inches (63.5 mm). It can operate in oxidizing atmospheres up to 1900oF (1038°C). It is one of the premier corrosion resistant materials in industrial applications.
Applications of Hastelloy C-276 Sheet:
- Chemical plant
- Petrochemical
- Flue gas desulfurization
- Pulp and paper industry
- Environmental protection
- Heat exchanger
- Flue gas desulfurization equipment
- Liquid corrosion resistant pump

Hastelloy c-276 sheet Chemical Analysis
| Nickel | Balance | Manganese | 1 |
| Molybdenum | 15.0 min.-17.0 max. | Carbon | 0.01 |
| Chromium | 14.5 min.-16.5 max. | Vanadium | 0.35 |
| Iron | 4.0 min.-7.0 max. | Phosphorous | 0.04 |
| Tungsten | 3.0 min.-4.5 max. | Sulfur | 0.03 |
| Cobalt | 2.5 | Silicon | 0.08 |
Mechanical Properties Of Alloy C276
| Properties | Metric | Imperial |
| Tensile strength (@thickness 4.80-25.4 mm, 538°C/@thickness 0.189-1.00 in, 1000°F) | 601.2 MPa | 87200 psi |
| Yield strength (0.2% offset, @thickness 2.40 mm, 427°C/@thickness 0.0945 in, 801°F) | 204.8 MPa | 29700 psi |
| Elastic modulus (RT) | 205 GPa | 29700 ksi |
| Elongation at break (in 50.8 mm, @thickness 1.60-4.70 mm, 204°C/@thickness 0.0630-0.185 in, 399°F) | 56% | 56% |
| Hardness, Rockwell B (plate) | 87 | 87 |
Hastelloy C276 Average Tensile Data
| Form | Condition | Test | Ultimate | Yield | Elongation |
| Temp., | Tensile | Strength at | in 2" percent | ||
| °F(°C) | Strength | 0.2% offset | |||
| ksi (MPa) | ksi (MPa) | ||||
| Sheet, 0.063 to 0.187" Thick |
Heat treated at | 400 (204) | 100.8 (695) | 42.1 (290) | 56 |
| 2050 °F | 600 (316) | 97.0 (669) | 37.7 (260) | 64 | |
| Rapid Quenched | 800 (427) | 95.0 (655) | 34.8 (240) | 65 | |
| 1000 (538) | 88.9 (613) | 33.8 (233) | 60 | ||
| Plate, 3/16 to 1.000" Thick |
Heat treated at | 400 (204) | 98.9 (682) | 38.2 (263) | 61 |
| 2050 °F | 600 (316) | 94.3 (650) | 34.1 (235) | 66 | |
| Rapid Quenched | 800 (427) | 91.5 (631) | 32.7 (235) | 60 | |
| 1000 (538) | 87.2 (601) | 32.8 (226) | 59 | ||
| Plate, 1.000" Thick |
Heat treated at | Room | 113.9 (785) | 52.9 (365) | 59 |
| 2050 °F | 600 (316) | 96.3 (664) | 36.2 (250) | 63 | |
| Rapid Quenched | 800 (427) | 94.8 (654) | 30.5 (210) | 61 |
Hastelloy C-276 (N10276) Physical Properties:
- Relative density 8.9g/cm3.
- Melting point 1025-17℃.
Hastelloy C276 Sheet Heat Treatment
- Annealing: ASME SB 575 UNS N10276 annealing temperature ranges from 1040°C (1900°F) to 1150°C (2100°F) followed by rapid quenching to room temperature.
- Solution Annealing: Solution annealing can be performed at a higher temperature (about 1175°C (2150°F)) followed by rapid cooling.
- Stress relief: When 2.4819 material is welded or formed, stress relief at around 760°C (1400°F) can reduce residual stress and enhance the dimensional stability of the material.
Machining ASTM B575 Hastelloy C276
Due to the toughness and work hardening tendency of nickel c276 plate, it is necessary to select suitable cutting tools: carbide cutting tools. The process needs to be slow and add coolant, etc.
ASTM B575 (C276) Hastelloy Hot forming
C-276 alloy hot forming is quenched immediately at 1150℃ and quenched with tap water. Cold deformation of C276 alloy will increase its compressive strength.
Suppliers Welding process
Such as gas tungsten arc welding (GTAW), gas metal arc welding (GMAW), arc welding or other welding processes.
FAQ
Q: About Hastelloy c276 sheet price per kg?
Q: How long does your delivery time take?
Q: Is There Sample Service?
Q: What Is The Minimum Order Quantity?
Q: How to pack the ASTM B575 N10276 products?
Q: Exported Countries
Hot Tags: hastelloy c276 sheet, hastelloy c276, 276 sheet, hastelloy sheet, din 2.4819
Previous
Hastelloy C22 SheetYou Might Also Like
Send Inquiry