Alloy 718 Seamless Tube
UNS N07718 (GH4169)
AMS 5589 seamless tube
OD 12.7-88.9 mm | WT 1.0-10 mm
Solution annealed / direct aged / double aged
Alloy 718 (UNS N07718; GH4169) is a precipitation-hardened nickel-iron-chromium alloy. Its strength does not come from the mill roller or from solid-solution chemistry - it comes from ordered γ″ (gamma double-prime) precipitates of Ni₃Nb that form only when the material is held through a controlled ageing cycle. That single sentence explains most of the procurement decisions on this page.
Table 1. Chemical composition (UNS N07718, weight %)
| Element | Range (%) | Role |
|---|---|---|
| Ni | 50.0–55.0 | Matrix; cryogenic toughness base |
| Cr | 17.0–21.0 | Oxidation resistance |
| Fe | balance | Cost control vs pure Ni grades |
| Nb + Ta | 4.75–5.50 | The γ″ former - the whole point of the alloy |
| Mo | 2.80–3.30 | Solid-solution support |
| Ti | 0.65–1.15 | Minor γ′ contribution |
| Al | 0.20–0.80 | Minor γ′ contribution |
| C | ≤ 0.08 | - |
Technical parameters: the size reality of 718 tube
Here is a check worth running on any listing that promises "seamless 718 tube, OD 6–219 mm": hot-rolled seamless tube in this alloy is genuinely produced in small-to-mid diameters and thin-to-moderate walls - think roughly 12.7 mm (1/2") up to around 88.9 mm (3.5") OD with walls from under 1 mm to about 10 mm.
Above that range, "tube" in practice means bar or forging stock machined and bored - a legitimate product, but it comes with bar-standard certificates (ASTM B637 / AMS 5662 territory), different inspection economics and different lead times.
Table 2. Form-to-document mapping for 718
| What you asked for | Document that actually governs it | Practical range |
|---|---|---|
| Seamless tube, thin wall | AMS 5589 (solution treated) | ~OD 12.7–88.9 mm |
| Larger "tube" / heavy wall | Machined from ASTM B637 or AMS 5662 bar/forging | OD above ~88.9 mm |
| Sheet-derived tube / fabricated | AMS 5590 sheet + welded and rolled | Project-specific |
| Flanges and fittings on 718 lines | B637-family bar/forging documents | Per machining drawing |
If a certificate cites a bar standard for something quoted as tube - or vice versa - that is not pedantry. The mechanical test frequency, ultrasonic requirements and tolerances differ between the document families, and your inspector will flag it at receiving.
Delivery condition: the decision that changes everything
This is the section the SERP pages skip, and it is where 718 tube quotes quietly diverge. Three delivery conditions exist, and they are not interchangeable:
Table 3. The three delivery conditions of Inconel 718 tube
| Condition | Thermal cycle | Typical 0.2% yield (RT) | Hardness | Buy it when |
|---|---|---|---|---|
| Solution annealed (AMS 5589 base) | ~955–980°C, rapid cool | ~450–500 MPa | ~≤ 36 HRC workable | You will cold-form, machine heavily, or weld before ageing |
| Direct aged | Age ~720°C / 8 h, controlled cool to ~620°C / 8 h | ~1030–1170 MPa | 38–44 HRC | Standard high-strength line service, no further hot work |
| Solution + double age (full) | Solution anneal, then 720/620°C two-stage age | ~1170–1250 MPa | ~40–44 HRC | Peak strength for pressure-bearing and tooling duty |
Three consequences follow from this table, and each one has cost money for somebody:
- You cannot easily machine aged 718. At 40+ HRC with abrasive γ″ in the matrix, tool life collapses. If your fabrication plan involves significant machining, buy annealed tube, machine it, then age - not the reverse. Buying aged tube "because stronger is better" and then battling it on a lathe is the most common self-inflicted cost on this alloy.
- Aged tube is dimensionally stable; annealed tube can move. Ageing at 720°C relieves and strengthens simultaneously, which is why precision-bore applications often order final-machined-after-age. If your supplier ages after final machining, expect small bore growth - specify the sequence in the PO, not in a phone call.
- Welding resets everything locally. A weld in annealed tube can be aged with the joint; a weld in fully aged tube creates an annealed HAZ and a re-precipitation story that needs its own procedure. This is a one-sentence flag here - the welding-filler and PWHT routing for 718 deserves its own conversation with whoever supplies you.
Performance boundaries: where 718 tube wins and where it stops
The service ceiling
The γ″ precipitates that make 718 strong are metastable. Hold the tube much above 650–700°C long-term and they coarsen; strength walks back down and never returns without a full re-solution cycle. Several listing pages quote "up to 700°C" without this caveat - the honest framing is: 718 tube is a superb material up to roughly 650°C continuous, tolerates short excursions above, and is the wrong long-term choice beyond that window (that is 625 or 740-class territory, by chemistry and by price).
The low end
This is the underrated direction. 718's austenitic matrix keeps toughness at cryogenic temperatures - published programme data extends to liquid-hydrogen service near -253°C - and yield actually increases as temperature drops. Cryogenic and aerospace pressure lines are a legitimate tube application, and a procurement manager who has only ever seen 718 described as "high temperature alloy" will miss that it is simultaneously a deep-cryogenic one. Few materials in this price class serve both ends.
Sour service
In H₂S-bearing environments, NACE MR0175/ISO 15156 governs 718 with a hardness ceiling of 40 HRC in the aged condition and associated yield restrictions depending on environment class. Two practical notes: the annealed condition is not automatically compliant - it is simply too soft to be listed as an approved high-strength state, and the compliance story lives in the aged condition within the HRC cap; and certificates for sour-service tube should state condition and hardness explicitly, because "718" alone is not a sour-service claim.
Application scenarios
The tube form of 718 concentrates in four duty classes, all driven by the same three properties (aged strength, cryogenic toughness, oxidation resistance to ~650°C):
- Hydraulic and control lines on drilling and completions tools - aged condition, small OD, high pressure
- Cryogenic lines and pressure components - annealed-then-aged routing for weldability, strength retained to -253°C
- Rocket and propulsion feed lines - the aerospace-native application, tight tolerances, full heat-treatment traceability
- High-strength instrumentation and sample lines where 625 tube lacks the yield and 316L lacks both
How to specify (and what it does to price)
A complete 718 tube specification is five fields, and every one of them moves price or risk:
- Alloy + UNS: Inconel 718 / N07718 (avoid bare "alloy 718" with no UNS on the PO)
- Document: AMS 5589 for seamless tube (or the machining-stock document if the item is bored bar)
- Size: OD × wall × length; state whether tolerance is per AMS or per your drawing
- Delivery condition: annealed / direct aged / solution + double age - with the hardness band expected
- Service flag: sour service or not - it changes certificate content, not just composition
FAQ
Q: About Alloy 718 tube price per kg?
A: Prices ranges from $25 to $40 per kg, vary depending on size, wall thickness, supplier etc.
Q: How long does your delivery time take?
A: Delivery time is within 5-21 days
Q: Is There Sample Service?
A: Samples Are Provided Free Of Charge
Q: What Is The Minimum Order Quantity?
A: No Minimum Order Quantity
Q: How to pack the products?
A: The inner layer has a waterproof paper outer layer and is fixed with a fumigation wooden pallet.
Q: Exported Countries
A: Brazil, South Africa, Indonesia, India, Singapore, Malaysia, Iran, Russia, UAE, Chile, Laos, etc
Hot Tags: N07718, AMS 5589, GH4169, aged condition, solution annealed, double age, gamma prime