Alloy 31 (UNS N08031) and 2507 super duplex stainless steel (UNS S32750) are often the ultimate choices for engineers. Alloy 31 pursues extreme corrosion resistance in single-phase austenite with ultra-high nickel, chromium and molybdenum content, while 2507 achieves a balance of ultra-high strength and corrosion resistance on an iron matrix through nitrogen alloying of the duplex structure.

 

Alloy 31 s32750 material supplier

HT PIPE is a leading stockist and global exporter with over 15 years of expertise in international trade. We supply pipes, astm b625 n08031 plates, astm a240 super duplex 2507 plate, round bars, and a comprehensive range of pipe fittings, flanges, and valves. Contact us now for free quotes and personalized product information.

 

alloy 31 and s32750 Corrosion Resistance comparison

General Corrosion Resistance

N08031: Excellent in H₂SO₄, H₃PO₄, organic acids (esp. contaminated). Superior HCl resistance vs. most SS/Ni alloys.

2507: Excellent in oxidizing acids (e.g., HNO₃). Limited in HCl; Moderate H₂SO₄ resistance.

 

Localized Corrosion Resistance

Alloy 31: PREN ≥ 43. Top-tier pitting/crevice resistance (hot chlorides, low pH). Excellent SCC resistance.

2507: PREN ≥ 42. Equally top-tier pitting/crevice resistance. Outstanding Cl⁻-SCC resistance.

 

alloy 31

Alloy 31 vs. 2507: Chemical Composition Comparison

Element Alloy 31 (UNS N08031) 2507 (UNS S32750)
Nickel (Ni) 30.0–32.0% 6.0–8.0%
Chromium (Cr) 26.0–28.0% 24.0–26.0%
Molybdenum (Mo) 6.0–7.0% 3.0–4.0%
Copper (Cu) 1.0–1.4% ≤ 0.5%
Nitrogen (N) 0.15–0.25% 0.24–0.32%
Iron (Fe) Balance Balance
Manganese (Mn) ≤ 2.0% ≤ 1.2%
Silicon (Si) ≤ 0.3% ≤ 0.8%
Carbon (C) ≤ 0.015% ≤ 0.03%
Phosphorus (P) ≤ 0.02% ≤ 0.035%
Sulfur (S) ≤ 0.01% ≤ 0.02%
Tungsten (W) – –

 

nickel alloy 31 vs 2507 Performance Comparison

Property Alloy 31 (N08031) 2507 (S32750)
Mechanical Strength YS (Rp0.2): ≥ 310 MPa; UTS (Rm): ≥ 650 MPa (Annealed) YS (Rp0.2): ≥ 550 MPa; UTS (Rm): ≥ 800 MPa (Annealed)
Toughness/Ductility Excellent (austenitic). High impact toughness, good cryogenic performance. Good but lower than austenitics. Ductile-brittle transition exists.
Weldability Good. Use matching filler (ERNiCrMo-11/12). Mind heat input. Good. Use filler (ER2594). Strict interpass T control (<100°C).
Formability (Cold/Hot) Austenitic. High work-hardening. Hot work with care. High strength/hardness → difficult cold forming. Narrow hot-working range (950–1150°C).
Thermal Stability Max service T: ~400–450°C (σ-phase risk above). Max service T: ~300°C (Avoid 475°C embrittlement & σ-phase).
Cost High (High Ni/Cr/Mo) Significantly lower than Alloy 31 (Fe-based, low Ni).

 

How to choose the suitable one?

Q: Faced with boiling concentrated sulfuric acid or highly concentrated hydrochloric acid?

A: Alloy 31 is your best choice.

 

Q: Designing ultra-high pressure vessels or large thin-walled structures?

A: The strength advantage of 2507 is irreplaceable.

 

Q: Is the medium high-temperature seawater or chlorinated oil and gas?

A: Both are good, and 2507 is cheaper.

 

Q: Operating temperature exceeds 300°C for a long time? 

A: Use 2507 with caution, Alloy 31 is safer.

 

Q: Extremely sensitive to budget and working conditions allow?

A: 2507 provides top duplex steel performance.

Contact now

 

 

Send Inquiry

whatsapp

Phone

E-mail

Inquiry